01. Steel

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

TIN

Monolayer

Ti, N

2400 HV

450 °C

600 °C

2.5 µm±0.5

0.55

TIN

Monolayer

Ti, N

2400 HV

450 °C

600 °C

2.5 µm±0.5

0.55

TIN

Monolayer

Ti, N

2400 HV

450 °C

600 °C

2.5 µm±0.5

0.55

TIN

Monolayer

Ti, N

2400 HV

450 °C

600 °C

2.5 µm±0.5

0.55

Monolayer

Ti, N

2400 HV

450 °C

600 °C

2.5 µm±0.5

0.45

Monolayer

Ti, N

2400 HV

450 °C

600 °C

2.5 µm±0.5

0.45

Monolayer

Ti, N

2400 HV

450 °C

600 °C

2.5 µm±0.5

0.45

Monolayer

Ti, N

2400 HV

450 °C

600 °C

2.5 µm±0.5

0.45

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.6

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.6

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.6

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.6

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.3

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.3

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.3

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.3

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

See file

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.3

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.3

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.3

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

See file

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.6

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.6

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.6

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.6

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.3

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.3

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.3

Monolayer

Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

See file

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm±0.5

0.2

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm±0.5

0.2

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm±0.5

0.2

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm±0.5

0.2

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

See file

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm±0.5

0.2

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm±0.5

0.2

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm±0.5

0.2

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm±0.5

0.2

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Bilayer

CrN + a-C:H:Me

2800 HV

450 °C

900 °C

2.5 µm±0.5

0.15

Bilayer

CrN + a-C:H:Me

2800 HV

450 °C

900 °C

2.5 µm±0.5

0.15

Bilayer

CrN + a-C:H:Me

2800 HV

450 °C

900 °C

2.5 µm±0.5

0.15

Bilayer

CrN + a-C:H:Me

2800 HV

450 °C

900 °C

2.5 µm±0.5

0.15

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

See file

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

CRN

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm ±0.5

0.3

CRN

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm ±0.5

0.3

CRN

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm ±0.5

0.3

CRN

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm ±0.5

0.3

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm±0.5

0.2

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm±0.5

0.2

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm±0.5

0.2

Monolayer

Cr, N

1800 HV

450 °C

800 °C

3 µm±0.5

0.2

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

VIC

Monolayer

a-C:H:Me

2000 HV

450 °C

400 °C

1.5 µm±0.5

0.15

VIC

Monolayer

a-C:H:Me

2000 HV

450 °C

400 °C

1.5 µm±0.5

0.15

VIC

Monolayer

a-C:H:Me

2000 HV

450 °C

400 °C

1.5 µm±0.5

0.15

VIC

Monolayer

a-C:H:Me

2000 HV

450 °C

400 °C

1.5 µm±0.5

0.15

Bilayer

CrN + a-C:H:Me

2800 HV

450 °C

900 °C

2.5 µm±0.5

0.15

Bilayer

CrN + a-C:H:Me

2800 HV

450 °C

900 °C

2.5 µm±0.5

0.15

Bilayer

CrN + a-C:H:Me

2800 HV

450 °C

900 °C

2.5 µm±0.5

0.15

Bilayer

CrN + a-C:H:Me

2800 HV

450 °C

900 °C

2.5 µm±0.5

0.15

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

See file

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

ZRN

Monolayer

Zr, N

2000 HV

450 °C

550 °C

2.5 µm±0.5

0.4

ZRN

Monolayer

Zr, N

2000 HV

450 °C

550 °C

2.5 µm±0.5

0.4

ZRN

Monolayer

Zr, N

2000 HV

450 °C

550 °C

2.5 µm±0.5

0.4

ZRN

Monolayer

Zr, N

2000 HV

450 °C

550 °C

2.5 µm±0.5

0.4

VIC

Monolayer

a-C:H:Me

2000 HV

450 °C

400 °C

1.5 µm±0.5

0.15

VIC

Monolayer

a-C:H:Me

2000 HV

450 °C

400 °C

1.5 µm±0.5

0.15

VIC

Monolayer

a-C:H:Me

2000 HV

450 °C

400 °C

1.5 µm±0.5

0.15

VIC

Monolayer

a-C:H:Me

2000 HV

450 °C

400 °C

1.5 µm±0.5

0.15

Bilayer

CrN + a-C:H:Me

2800 HV

450 °C

900 °C

2.5 µm±0.5

0.15

Bilayer

CrN + a-C:H:Me

2800 HV

450 °C

900 °C

2.5 µm±0.5

0.15

Bilayer

CrN + a-C:H:Me

2800 HV

450 °C

900 °C

2.5 µm±0.5

0.15

Bilayer

CrN + a-C:H:Me

2800 HV

450 °C

900 °C

2.5 µm±0.5

0.15

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

See file

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradiente

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

See file

See our list of coatings