PVD Coatings / Cutting Tools

Carving

Metal Estalki has developed a family of coatings that improve performance thanks to their high resistance to impact and thermal shock, i.e. hot hardness, chemical inertness and high oxidation resistance.

Hobbing cutter edge with rounded cutting edge and coated

PVD Coatings for Carving

01. HSS hob

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

TIN

Monolayer

Ti, N

2400 HV

450 °C

600 °C

2.5 µm±0.5

0.55

TIN

Monolayer

Ti, N

2400 HV

450 °C

600 °C

2.5 µm±0.5

0.55

TIN

Monolayer

Ti, N

2400 HV

450 °C

600 °C

2.5 µm±0.5

0.55

TIN

Monolayer

Ti, N

2400 HV

450 °C

600 °C

2.5 µm±0.5

0.55

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Monolayer

Al, Ti, N

3800 HV

450 °C

800 °C

2.5 µm±0.5

0.6

Multinanogradient

Ti, Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.25

Multinanogradient

Ti, Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.25

Multinanogradient

Ti, Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.25

Multinanogradient

Ti, Al, Cr, N

4200 HV

450 °C

1000 °C

3.5 µm±0.5

0.25

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

See file

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Multinanogradient

Al, Ti, Si, N

4500 HV

450 °C

1200 °C

2.5 µm±0.5

0.3

Designation

Structure

Components

Nanohardness

Process temperature

Max. working temperature

Thickness

Coef. friction

See file